SpoolBoss.
All guides

Guides / Print quality

How to fix warping and corners lifting off the bed

Corners curling up mid-print ruin parts and can knock prints loose. Here is why warping happens and the practical fixes that keep your prints flat.

November 22, 2026 · 4 min read · By the SpoolBoss team

Close-up of a nozzle printing a first layer

You come back to a print and one corner has peeled up like an old sticker. Sometimes it is just a cosmetic curl, sometimes the part pops loose and the nozzle drags it across the bed. Warping is one of the most common FDM problems, and the good news is that it follows simple physics. Once you understand why it happens, the fixes are mostly a matter of working through a short list in the right order.

Why prints warp in the first place

Hot plastic shrinks as it cools. Each new layer is laid down warm on top of a layer that has already cooled and shrunk, so the top pulls inwards on the bottom. That pull builds up layer after layer.

Corners suffer most because the stress from two edges meets there, and a sharp corner has very little contact area holding it down. When the pull beats the grip on the bed, the corner lifts.

So every fix does one of two things: reduce the shrinking stress, or increase the grip. Large flat parts and materials that shrink more, such as ABS, ASA and nylon, need both.

Start with grip: a clean, well-prepared bed

Fingerprints are the most common hidden cause. The oil from one touch is enough to stop a corner sticking. A good first layer matters just as much, and our first-layer guide covers levelling and squish in detail, so check that before going further.

For textured or smooth PEI, wash the plate with warm water and a drop of washing-up liquid, rinse well and dry with a clean towel. Wipe with isopropyl alcohol between prints. Handle the plate by its edges.

If a clean bed still is not enough, a thin layer of glue stick helps many materials. With PETG on smooth PEI, glue stick also works as a release layer, because PETG can bond so well it tears the surface.

Hands servicing a 3D printer toolhead
A tidy, draught-free corner of the workshop goes a long way towards keeping prints flat on the bed.

Get temperatures and cooling right

A warm bed keeps the bottom layers soft enough to relax instead of pulling free. Typical bed temperatures are below, but check the filament maker's guidance and adjust in 5 °C steps.

Part cooling is the other half. Turn the fan off for the first two or three layers so they bond well. For ABS and ASA, keep the fan low or off for most of the print, because fast cooling is exactly what drives shrinkage.

Draughts matter more than most people think. An open window, air conditioning or a fan blowing across the printer will cool one side faster and lift those corners first. An enclosure, even a simple cover, keeps the air around the print warm and still. ABS and ASA give off fumes while printing, so run them in a well-ventilated room or with an enclosure that is vented or filtered.

  • PLA: bed around 50 to 65 °C
  • PETG: bed around 70 to 85 °C
  • ABS and ASA: bed around 90 to 110 °C, ideally enclosed
  • Nylon: often 70 to 100 °C or more, depending on the blend
SymptomLikely causeFix
One corner lifts, always the same sideDraught or uneven bed heatBlock air flow, add an enclosure, check bed heats evenly
All corners lift slightly on large partsToo much shrink stressAdd a brim, lower infill, round the corners
Part pops off the bed completelyPoor adhesion or dirty bedWash the bed, re-check first layer, try glue stick
Lifting starts after a few layersPart cooling fan too strongLower fan speed, especially for ABS and ASA
Edges curl on ABS or ASA onlyCold air around the printUse a ventilated enclosure and a hotter bed

Brims, mouse ears and smarter design

A brim adds a thin skirt of extra plastic stuck to the part's edge, giving the corners much more area to hold onto. A width of 5 to 10 mm suits most parts. It peels or trims off afterwards.

If a full brim is a pain to clean up, add small discs, often called mouse ears, under just the corners. Many slicers can place them for you, or you can model them as 0.2 to 0.4 mm thick circles.

When you control the design, round or chamfer sharp outside corners, since even a 2 to 3 mm radius spreads the stress. Lower infill on large flat parts reduces how much plastic is shrinking. Where possible, orient the part so the largest flat area is not also the longest dimension sitting on the bed.

A checklist for stubborn warping

Change one thing at a time and print a small test part with sharp corners, so you know which change actually helped.

Keep an eye on the first part of each test print. Lifting usually starts early, and catching it then saves filament. As always, follow the usual precautions if a print runs while you are away from the room.

  1. Wash the bed with soap and water, then stop touching the print surface.
  2. Re-check your first layer height and squish.
  3. Raise the bed temperature by 5 °C, staying within the filament maker's range.
  4. Turn part cooling off for the first layers and lower it overall for ABS and ASA.
  5. Remove draughts or add an enclosure, with ventilation for ABS and ASA.
  6. Add a brim or mouse ears.
  7. Round the corners or reduce infill if you can edit the model.
  8. Dry the filament, since damp filament can weaken bed adhesion.
Every warping fix does one of two things: it reduces the shrinking stress, or it increases the grip.

Keep a record of what works

Once you find the settings that hold a material flat, write them down per printer and per filament. It saves repeating the same tests next time a corner lifts.

If you want help working out what went wrong, SpoolBoss is a free app with an AI print doctor that can diagnose a failed print from a photo, and it keeps track of your printers and spools alongside it.

Common questions

Why does warping happen more with ABS than with PLA?

ABS shrinks more as it cools and prints at a higher temperature, so the gap between the hot nozzle and room air is larger. A hotter bed, little or no part cooling and an enclosure help, and you should always print it with good ventilation.

Can I fix a part that has already warped?

Not reliably. Minor curl on PLA can sometimes be eased flat with gentle heat, but the part will rarely be accurate again. It is usually better to fix the cause and reprint.

Is a brim always needed?

No. Small parts and most PLA prints on a clean, well-levelled bed are fine without one. Use a brim for large flat parts, sharp corners or high-shrink materials.

Free on phone and computer

Try it on your own printers.

SpoolBoss tracks printers, filament, queue and costs.

Open SpoolBoss

Keep reading

More guides