SpoolBoss.
All guides

Guides / Print quality

How to stop stringing on 3D prints

Stringing leaves fine hairs between parts of a print. Here is how to fix it with temperature, retraction and travel settings, one change at a time.

November 20, 2026 · 4 min read · By the SpoolBoss team

Close-up of a nozzle printing a first layer

Stringing is the web of thin plastic hairs that appears between separate parts of a print, like the gap between two towers. It happens when molten filament oozes from the nozzle while the print head moves across open air. The good news is that it is one of the easier faults to fix once you know which settings matter and test them in a sensible order.

Why stringing happens

Whenever the nozzle stops extruding and travels to a new spot, the plastic inside the hot end is still liquid. Pressure and gravity push a little out. If enough leaks during the move, it stretches into a string that cools and stays on the part.

Four things drive this: moisture in the filament, nozzle temperature, retraction settings and how the slicer plans travel moves. Work through them in that order, because the first two are the most common causes and the quickest to rule out.

Check the filament and the temperature first

Damp filament is a leading cause, especially with PETG, nylon and TPU. Water in the plastic turns to steam in the nozzle and forces out extra material during travel. If you hear popping or see a rough, bubbly surface, dry the spool before touching any other setting. Our article on keeping filament dry covers how.

Next, look at temperature. Hotter plastic is runnier and oozes more. Many people print at the top of the range on the spool label without needing to. Print a temperature tower, which steps the temperature down every few millimetres, and pick the lowest setting that still gives good layer bonding and a clean surface.

As a rough guide, PLA usually runs between 190 and 220 °C, PETG between 220 and 250 °C, and ABS or ASA between 230 and 260 °C. Always check the maker's guidance for your filament, as blends vary.

Spools of filament stored in a clear box
Small test prints make it quick and cheap to find the settings that stop stringing.

Tune retraction properly

Retraction pulls the filament back slightly before a travel move so less plastic sits ready to leak. Two settings matter: distance and speed. The right values depend heavily on your extruder type, so start from your printer maker's profile.

Typical starting ranges are 0.5 to 2 mm for direct drive extruders and 3 to 7 mm for Bowden setups, with speeds of around 25 to 45 mm/s. Too much retraction can grind the filament or cause clogs, so increase it in small steps.

  1. Print a small retraction test, such as two thin towers spaced a few centimetres apart.
  2. Leave temperature fixed and raise retraction distance by 0.5 mm for direct drive, or 1 mm for Bowden, per test.
  3. Stop when the strings disappear or become thin wisps that brush off easily.
  4. Then adjust retraction speed by 5 mm/s in either direction to see if it cleans up the last few strings.
  5. Save the result as a profile for that filament, since another brand may need different values.
SymptomLikely causeFix
Many fine hairs between partsNozzle too hotPrint a temperature tower and lower by 5 °C steps
Strings plus popping and rough surfaceDamp filamentDry the spool, then retest
Thick strings and blobs at travel endsRetraction too short or slowIncrease distance in small steps, then tune speed
Strings got worse after raising retractionToo much retraction or heat creepReduce distance and check hot end cooling
Strings only on long open movesSlow travel or poor path planningRaise travel speed and enable avoid crossing perimeters
Grinding noise and gaps after retraction changesFilament chewed by extruderLower retraction distance and speed, check tension

Use the slicer's travel settings

If strings remain after tuning retraction, change how the nozzle moves. Faster travel gives the plastic less time to ooze, and smarter paths avoid crossing open air at all.

Most slicers offer the options below, though names differ between programs.

  • Raise travel speed, often to 150 mm/s or more if your machine handles it well.
  • Turn on avoid crossing perimeters or combing so the nozzle stays over the printed part.
  • Enable wipe, which drags the nozzle across the part before travel to clean the tip.
  • Set a minimum travel distance for retraction so very short moves do not retract needlessly.
  • Use Z hop sparingly, as it helps with nozzle scraping but can add stringing.
Pick the lowest temperature that still bonds your layers well, and much of the stringing goes with it.

Material quirks and cleaning up

PETG strings more than most materials and rarely becomes perfectly clean. Aim for fine wisps rather than none. TPU and other flexible filaments need very short, slow retraction, or none, as they buckle in the extruder; rely more on lower temperature and travel settings. ABS and ASA give off fumes, so print them in a well-ventilated space or an enclosure with filtration.

Light strings on a finished part can be removed with a quick pass of a heat gun on a low setting. Keep it moving, work in short bursts and let the part cool between passes so thin walls do not sag. A craft knife or fine file handles thicker blobs.

When strings appear suddenly on a profile that used to work, think about what changed: a new spool, damp weather or a worn nozzle. If you track your spools and print hours in SpoolBoss, you can photograph the failed print and let the AI print doctor suggest likely causes, which is a handy second opinion before you start changing settings.

Common questions

Can I get PETG completely string-free?

Rarely. PETG is naturally stringy. Dry filament, a lower temperature and good travel settings will usually reduce it to light wisps that brush off or vanish with a quick pass of a heat gun.

Should I change several settings at once to save time?

No. If you change temperature, retraction and travel together, you will not know which one helped or made things worse. Change one setting per test print and note the result.

Why did stringing start on a profile that worked before?

The usual suspects are a new or damp spool, a different filament brand, or a worn or partly clogged nozzle. Dry the filament and check the nozzle before retuning your slicer.

Free on phone and computer

Try it on your own printers.

SpoolBoss tracks printers, filament, queue and costs.

Open SpoolBoss

Keep reading

More guides